Home » Questions » Half Log Siding » Archive-2682

Archive-2682

383 viewsHalf Log Siding

bought a 9 yrs.old log home that had been stained with cwf-uv(redwood) every 3 yrs. and never cleaned or washed. we have owned for 6 yrs. and are going to restain. We appliedbleach and pressure washed. Some natural wood showing most of house still looks stained. Does it matter? What is the best stain?Does it need to be corn blasted?can you use a stripping agent?Can we just restain? Painter wants to strip with pressure washer and just stain over.I need log help in N.C.

If you pressure wash I would wait about 1-2 months before staining to allow to dry out properly. Life Line Stain by Perma Chink is one of the best.